Ok it's not the first time someone has had a spinning insert in their tank. Why??? Galvanic corrosion. A steel bolt in a brass insert spells disaster. The steel bolt will corrode far faster than the insert causing the bolt to seize in the insert. What a pain in the ass. I actually had one seize got it out and bonded the insert back in. 3 months later the tank is now leaking fuel. Gmx tank here I come. It's retarded that I should need to pull the bolts every month to clean the threads and reapply a corrosion resistant substance.
My solution.... How about use a bolt made from UHMW or some other non metalic material? UHMW is super strong. I have a rod of it I use as a damm punch. Worst case you ez out the bolt if ypu snap the head off.